http://repositoriodigital.ipn.mx/handle/123456789/11459| Título : | Structural and morphology comparison between m-LaVO4 and LaVO3 compounds prepared by sol-gel acrylamide polymerization and solid state reaction |
| Palabras clave : | Ceramics Sol–gel processes |
| Fecha de publicación : | 16-ene-2013 |
| Editorial : | elservier |
| Descripción : | We contrast the production of LaVO3 polycrystalline samples obtained by reduction of m-LaVO4 prepared by sol–gel acrylamide polymerization (SGAP) and solid state reaction (SSR). For SGAP the formation of m- LaVO4 occurs at 400 ◦C, for SSR at 1400 ◦C. For m-LaVO4-SGAP we observe a homogeneous morphology with needle-shaped grains of 50nm average size. The SSR presents a broader size distribution in the micrometer range. Both m-LaVO4 samples were reduced into LaVO3 using a Zr rod at 850 ◦C in vacuum. LaVO3-SGAP presents a homogeneous grain distribution with an average size of 745 nm. LaVO3-SSR has an average size of 3.45 m. The stoichiometry of all compoundswas confirmed by energy dispersive X-ray spectroscopy. X-ray powder diffraction and transmission electron microscopy give crystal structures in agreement with those reported in the literature. |
| URI : | http://www.repositoriodigital.ipn.mx/handle/123456789/11459 |
| Otros identificadores : | http://hdl.handle.net/123456789/979 |
| Aparece en las colecciones: | Doctorado |
Ficheros en este ítem:
| Fichero | Descripción | Tamaño | Formato | |
|---|---|---|---|---|
| RESUMEN LaVO3.docx | 13.05 kB | Microsoft Word XML | Visualizar/Abrir |
Los ítems de DSpace están protegidos por copyright, con todos los derechos reservados, a menos que se indique lo contrario.